The catalyst matrix.
Seventeen grades across five families, each defined by the production problem it solves. All grades are addition-cure platinum catalysts supplied with TDS and batch COA. Concentrations run from 1,500 to 5,000 PPM, including the 3,000 PPM platinum catalyst most often used to balance cure speed against catalyst cost.
Standard Karstedt's Catalysts
PC-11 to PC-16 form the volume backbone of the range: high-purity Karstedt's catalyst in six platinum concentrations from 1,500 to 5,000 PPM, all at 400–500 cP and compatible with the full inhibitor range. These are the grades most commonly used for general-purpose compounding, moulding and high-precision coating lines, and the ones we recommend when a formulation is being matched from an existing supplier.
1,500 PPM
The general-purpose grade. 1,500 PPM is the most widely used concentration for large-volume silicone compounding, where a predictable cure at moderate catalyst cost matters more than speed.
5,000 PPM
The high-concentration workhorse. 5,000 PPM delivers fast cross-linking for lines that need short cycle times, and it is the grade most often specified for injection and rapid-cure processes.
3,000 PPM
The middle grade, chosen when 1,500 PPM is too slow and 5,000 PPM is more catalyst than the formulation needs. A common starting point for balancing cure speed against raw-material cost.
High-Activity & Anti-Poisoning Catalysts
PC-41 to PC-46 mirror the standard concentration grades but with enhanced catalytic activity and improved resistance to substrate contaminants. They are the practical choice when a line runs below ideal conditions — recycled filler, variable cure ovens, long pot life between mixing and shaping — and curing failures are costing yield rather than indicating a formulation fault.
1,500 PPM
The 1,500 PPM high-activity grade: standard-range platinum loading with upgraded catalytic performance and better tolerance of substrate contaminants.
3,000 PPM
High-activity grade at 3,000 PPM, used where an existing 3,000 PPM formulation is fast enough on paper but not in the plant.
4,000 PPM
High-activity 4,000 PPM grade for automated lines that need a fast, repeatable cure onset and cannot afford start-up scrap.
Thermal Stability & Anti-Yellowing Catalysts
This is the differentiated part of the range. PC-42 holds colour below 100°C for long dwell times, while PC-50 and PC-51 remain stable above 150°C and can lift the heat resistance of the whole compound — methyl silicone toward phenyl performance, phenyl toward fluoro. These grades are specified into PPF top coats, optical films and high-temperature moulded parts.
5,000 PPM
The anti-yellowing benchmark. Under 85°C / 48 h accelerated aging, PC-42 holds ΔE 0.8 against 4.2 for a conventional Karstedt's catalyst. Specified into premium PPF top coats, optical films and any coating judged by colour after heat exposure.
Custom (1,000–20,000 PPM)
Ultra high-temperature grade with a low-viscosity profile (5–50 cP) for easy dispersion. Remains stable above 150°C for long dwell times, for thick sections and hot-running parts.
Custom (1,000–20,000 PPM)
The heat-resistance upgrade grade. Beyond its own thermal stability, PC-51 lifts the heat resistance of the whole compound: methyl silicone toward phenyl performance, phenyl toward fluoro. Used where the part specification is set by heat aging.
Advanced Anti-Poisoning Catalysts
Catalyst poisoning is one of the least visible causes of a non-curing batch. PC-18B is the first-generation grade for environments with slight to moderate poisoning agents, and PC-18A is the second generation, engineered against high concentrations and multiple contaminant types. PC-18A is under final R&D and available for evaluation samples only.
Custom (1,000–20,000 PPM)
First-generation anti-poisoning catalyst. Retains stable vulcanisation activity in environments with slight to moderate poisoning impurities — trace sulfur, phosphorus and nitrogen compounds.
Custom (1,000–20,000 PPM)
Second-generation anti-poisoning catalyst, engineered against high concentrations and multiple contaminant types. Under final R&D: available for evaluation samples, with commercial supply not yet committed.
Optical Grade High-Refractive-Index Catalysts
GZ-5 is formulated for high-refractive and phenyl silicone systems, where a conventional catalyst can cloud the compound or drop out of solution. Refractive index above 1.50, 400–800 cP, and a fully soluble profile make it the standard choice for Mini LED encapsulation and optical bonding.
Model list.
Open any grade for the full specification, dosage guidance and the inhibitor pairing recommendation.
1,500 PPM
The general-purpose grade. 1,500 PPM is the most widely used concentration for large-volume silicone compounding, where a predictable cure at moderate catalyst cost matters more than speed.
5,000 PPM
The high-concentration workhorse. 5,000 PPM delivers fast cross-linking for lines that need short cycle times, and it is the grade most often specified for injection and rapid-cure processes.
3,000 PPM
The middle grade, chosen when 1,500 PPM is too slow and 5,000 PPM is more catalyst than the formulation needs. A common starting point for balancing cure speed against raw-material cost.
4,000 PPM
High-activity grade for automated production lines, where consistent cure start and short residence time reduce scrap at start-up and shut-down.
2,000 PPM
The default grade for industrial silicone moulding. 2,000 PPM sits between the economy and high-speed grades and is the grade most often used to match an existing moulding formulation.
4,000 PPM-1
A batch-controlled 4,000 PPM grade for high-precision coating lines. The -1 suffix denotes the tight-tolerance batch configuration used where coat weight and cure are measured, not estimated.
1,500 PPM
The 1,500 PPM high-activity grade: standard-range platinum loading with upgraded catalytic performance and better tolerance of substrate contaminants.
3,000 PPM
High-activity grade at 3,000 PPM, used where an existing 3,000 PPM formulation is fast enough on paper but not in the plant.
4,000 PPM
High-activity 4,000 PPM grade for automated lines that need a fast, repeatable cure onset and cannot afford start-up scrap.
2,000 PPM
The 2,000 PPM high-activity grade for moulding shops whose cure is borderline: standard activity is technically sufficient, but yield improves with more robust kinetics.
4,000 PPM-1
Batch-controlled high-activity 4,000 PPM grade for precision coating lines, matching the PC-16 tolerance profile with enhanced kinetics.
5,000 PPM
The anti-yellowing benchmark. Under 85°C / 48 h accelerated aging, PC-42 holds ΔE 0.8 against 4.2 for a conventional Karstedt's catalyst. Specified into premium PPF top coats, optical films and any coating judged by colour after heat exposure.
Custom (1,000–20,000 PPM)
Ultra high-temperature grade with a low-viscosity profile (5–50 cP) for easy dispersion. Remains stable above 150°C for long dwell times, for thick sections and hot-running parts.
Custom (1,000–20,000 PPM)
The heat-resistance upgrade grade. Beyond its own thermal stability, PC-51 lifts the heat resistance of the whole compound: methyl silicone toward phenyl performance, phenyl toward fluoro. Used where the part specification is set by heat aging.
Custom (1,000–20,000 PPM)
First-generation anti-poisoning catalyst. Retains stable vulcanisation activity in environments with slight to moderate poisoning impurities — trace sulfur, phosphorus and nitrogen compounds.
Custom (1,000–20,000 PPM)
Second-generation anti-poisoning catalyst, engineered against high concentrations and multiple contaminant types. Under final R&D: available for evaluation samples, with commercial supply not yet committed.
Custom (1,000–20,000 PPM)
High-refractive-index catalyst for phenyl and high-RI silicone systems. RI above 1.50, complete molecular solubility, zero turbidity or precipitation. The grade behind our Mini LED encapsulation data.
Custom and on-request grades.
PC-47 to PC-49 are configured to order; specifications are confirmed before quotation. Concentrations outside 1,000–20,000 PPM are quoted per request.
Every quoted grade ships with a batch COA stating the measured platinum content.
Choosing a grade.
What is the difference between PC-11 to PC-16 and PC-41 to PC-46?
PC-41 to PC-46 mirror the concentration grades of PC-11 to PC-16 but with enhanced catalytic activity and improved resistance to substrate contaminants. Start with the standard series when the line is well controlled, and move to the high-activity series when cure failures correlate with filler or oven variation.
How do I choose a platinum concentration?
Concentration is matched to line speed, section thickness and inhibitor dosage — not to a quality tier. 1,500–2,000 PPM suits cost-sensitive compounding, 3,000–4,000 PPM is the common balance, and 5,000 PPM is used where fast cross-linking or very short cycles are required.
Can the concentration be customised?
Yes. Custom concentrations from 1,000 to 20,000 PPM are supplied to order, with the platinum content verified by ICP-OES and stated on the batch COA.
Which inhibitor should be paired with a catalyst?
For medium-high temperature cure use PC-611 or PC-612; for ambient cure use PC-613 or PC-614; for high-efficiency non-hazardous inhibition use PC-617; for high-refractive systems use GZ-612 or GZ-617.
Request a sample or get a quote
Tell us the grade, target PPM and application. Our technical team replies within 24 hours with a recommended grade and sample lead time.