Pot life is a setting, not a guess.
The catalyst decides how fast the compound cures; the inhibitor decides how long you can work with it. Seven grades cover pot life extension for ambient cure, medium-high temperature cure, high-efficiency alkynol chemistry and high-refractive systems. Where a low temperature silicone curing catalyst is needed, PC-613 and PC-614 keep the mixed batch workable at room temperature for minutes to hours instead of days.
Silicone curing inhibitor pot life extension is the job of this range: the inhibitor holds the platinum catalyst dormant until the part reaches cure temperature.
Working time and cure speed, decoupled.
An inhibitor reversibly blocks the platinum centre. While the compound is below the activation window the catalyst stays dormant; once the part reaches temperature the inhibitor releases and cure proceeds at full speed. The result is a long, controllable pot life without a slow cure.
- Set pot life from minutes to one week
- Hot cure speed essentially unchanged
- Dosage 0.1%–1.0% for standard types, 0.01%–0.20% for alkynol types
- For high-RI optics, use GZ-612 or GZ-617 with GZ-5
| Below activation | Inhibited, workable |
| At activation temperature | Rapid cross-linking |
| Over-dosage | Soft cure or tacky surface |
| Under-dosage | Short bath life, scorch risk |
Seven grades, four cure windows.
Open a grade for its cure behaviour, appearance, recommended dosage and the catalysts it pairs with.
Medium-to-high temperature
The default inhibitor for medium-to-high temperature cure systems. Buys bench and line time without slowing the cure once the part reaches temperature.
Medium-to-high temperature
For plants that need a full week of pot life and still want the same hot cure. Same dosage window as PC-611, longer open time.
Ambient / low temperature
For ambient-cure systems and heat-sensitive substrates. Lets the compound cure in minutes to hours at room temperature without an oven.
Ambient / low temperature
Ambient-cure inhibitor with a longer hold and lower viscosity than PC-613, for formulations that need more working time at room temperature.
High efficiency, non-hazardous
A silicone-modified alkynol inhibitor: strong inhibition at a tenth of the usual dosage, non-hazardous, and a crisp cure at about 140°C. Best cost-performance in the range.
High-RI systems
Inhibitor for high-RI systems that need low-to-medium temperature cure. Designed to pair with GZ-5 without clouding the optical compound.
High-RI systems
High-RI version of the alkynol inhibitor: strong inhibition, non-hazardous, and a complete cure at elevated temperature for optical systems built on GZ-5.
Which inhibitor for which process.
Medium-to-high temperature cure
Cure starts above 80°C and accelerates above 100°C, with room-temperature pot life from hours to a full week.
Ambient and low-temperature cure
Complete vulcanisation within minutes to hours at room temperature — for heat-sensitive substrates and ambient-cure systems.
High efficiency, non-hazardous
Silicone-modified alkynol chemistry: strong inhibition at 0.01%–0.20%, non-hazardous, complete cure at about 140°C.
High-refractive-index systems
Optical modifiers for phenyl systems, designed to pair with GZ-5 without clouding the compound.
Catalyst and inhibitor are one system.
A catalyst sample without the matching inhibitor is only half a trial. We supply paired samples so the first test in your lab reflects the real process.
Share the process
Cure temperature, line speed, target pot life and current issue.
Get a paired recommendation
Catalyst grade, PPM and inhibitor type with starting dosages for both.
Trial both components
Samples of catalyst and inhibitor arrive together for a representative test.
Lock the ratio
Confirm dosage against your cure oven and batch size, then scale.
Not sure which inhibitor to pair?
Send the catalyst grade and the pot life you need. We will reply with an inhibitor recommendation, dosage range and sample plan.