PPF top coat: ΔE 0.8 where the incumbent measured 4.2
A paint protection film top coat compared against its incumbent catalyst in the same accelerated aging run.
Each figure is tied to a measurement, and the result section below states the conditions that produced it. Field data and accelerated aging data are labelled separately, and the disclosure at the end of the case states how the data was obtained.
Measured, not claimed.
Schematic of the measurement behind this case: the same conditions, drawn to be read at a glance. The drawing is illustrative; the measured values are the ones stated in the result sections.
Where this grade is used.
Representative production images of the processes these grades are specified for. The parts shown are end applications, not test data; measured values stay in the data sections above.

The challenge.
A TPU paint protection film yellowed within the warranty period under combined solar UV and engine heat. The incumbent catalyst measured ΔE 4.2 after 48 h at 85°C — visible to the eye and outside specification.
The incumbent was tested in the same run, which is what makes the two ΔE figures directly comparable. Running both catalysts under one set of oven conditions removes the batch-to-batch variation that makes separate tests hard to read.
The film's failure is cosmetic first and functional later: customers see the colour change before they measure it, and the specification is written in ΔE because visual judgement does not hold across suppliers.
The solution.
PC-42 anti-yellowing catalyst in the top coat, with PC-611 inhibitor for line stability on the slot-die coater.
Dosage stayed inside the normal 0.05%–0.5% window. The change was the grade, not the loading: colour retention comes from the catalyst chemistry, and adding more of a conventional catalyst does not buy the same result.
PC-611 kept the slot-die bath stable through the run. On a coating line the inhibitor is part of the colour result, because a change in working time changes coat weight and therefore the optical path of the film.
The result, and what produced it.
The numbers at the top of the page are the headline metrics from this case. The paragraphs here explain what produced them, with the test method and the exposure stated alongside.
The reformulated top coat measured ΔE 0.8 after 85°C / 48 h against 4.2 for the incumbent, with no visible yellowing and mirror gloss retained in the customer's assessment. Colour difference was measured against an unstressed reference film.
The result is an accelerated-aging comparison with customer line validation. It is a screening result for formulation decisions, not a prediction of warranty life or field durability.
Accelerated aging accelerates one mechanism; it cannot reproduce every combination of UV dose, heat cycling and chemical exposure a film meets in service. Use the ΔE comparison to choose a grade, then validate on the vehicle programme's own cycle.
Accelerated aging at 85°C for 48 h, colour difference measured against unstressed reference film; comparison catalyst tested in the same run.
Internal accelerated aging comparison, with customer line validation.
The grades and the application behind this case.
Every case is tied to a catalyst grade and to an application page. The grade page carries the full specification; the application page carries the process window, dosage range and inhibitor pairing for this class of part.
| Model | Pt concentration | Viscosity | Recommended dosage |
|---|---|---|---|
| PC-42 | 5,000 PPM | 300–500 cP | 0.05%–0.5% of total compound |
| PC-50 | Custom (1,000–20,000 PPM) | 5–50 cP | 0.05%–0.5% of total compound |
Open a model for packaging, shelf life, features and inhibitor pairing. Where a case names more than one grade, the solution section states which one was used in the reported trial.
PPF & Coatings
Zero yellowing under engine heat and solar UV.
Optical-grade platinum catalysis for TPU and PET paint protection film top coats and adhesive modification.
Other problems, measured the same way.
Each case is structured identically, so the challenge, solution and result can be compared across industries with the same reading discipline.
Battery pack seal: VOC compliance without losing compression set
A battery pack seal was built on a peroxide cure system. VOC emissions failed the customer's incoming specification, and the alternative addition-cure trial produced uneven cell structure and compression set above the 10% limit.
Medical LSR diaphragm: 100 steam cycles without yellowing
A respiratory valve diaphragm had to survive repeated 121°C wet-heat sterilisation without visible colour change. With the incumbent catalyst, yield after sterilisation was 82% and rejected parts were discoloured.
Mini LED encapsulation: 99.82% transmittance at 95% yield
A high-refractive-index encapsulation compound clouded when the catalyst was added, and the resulting light scattering failed the transmittance target. Yield was limited by optical rejects rather than by the dispenser.
Run a comparable trial on your own line.
Send the part, the failure and the acceptance test. We will send evaluation samples of the grade used in this case, paired with the matching inhibitor, and confirm the starting dosage for your cure window.