Applications / Automotive

Zero yellowing under engine heat and solar UV.

Optical-grade platinum catalysis for TPU and PET paint protection film top coats and adhesive modification.

AutomotivePC-42 · PC-50 · PC-51 Process data included
Failure mode

Where the process breaks down.

Paint protection film is judged years after it leaves the line. The defect that ends a warranty claim is rarely a cure failure; it is a slow colour shift. The top coat yellows, the film hazes, and the change usually appears first at edges and on horizontal panels where heat and UV accumulate. A conventional Karstedt's catalyst cures the film perfectly well and still fails this test.

The mechanism is thermo-oxidative rather than kinetic, so raising catalyst loading or oven temperature does not restore colour once the film has aged. The formulation has to be protected at the catalyst level: a grade that holds colour through long dwell times below 100°C, and a thermal grade where the part itself runs hot.

Symptoms on the line

What the defect looks like.

  • Film yellows and hazes after months of sun exposure and engine-bay heat radiation
  • Colour drift shows first at the edges and on horizontal panels, then spreads
  • Conventional catalyst fails the ΔE requirement before the film reaches end of warranty
Solution

What the formulation needs.

PC-42 is formulated to hold colour below 100°C for long dwell times, and it is the grade our PPF customers specify when the acceptance criterion is measured colour rather than visual judgement. PC-50 and PC-51 extend the thermal envelope to 150°C and above for top coats that see more heat.

PC-42 is the grade most PPF customers specify when the acceptance criterion is a measured colour difference rather than a visual judgement. PC-50 and PC-51 extend the thermal envelope above 150°C where the top coat or the substrate underneath reaches higher temperatures.

On a slot-die line the catalyst is only half the system. PC-611 or PC-612 at 0.1%–1.0% keeps the coating bath stable through the run without slowing cure once the film reaches oven temperature. Dosage stays inside the normal 0.05%–0.5% window and is set against line speed, not against colour.

Trial plan

How the first evaluation is run.

  • Start from PC-42 unless the failure mode points to another grade.
  • Hold catalyst dosage at the lower bound of 0.05%–0.5% and fix the inhibitor dose.
  • Run the customer acceptance test on the cured part, not on the liquid mix.
  • Change one variable per run: grade, dosage or inhibitor.
Field data

What the numbers behind this page show.

ΔE 0.8
after 85°C / 48 h vs 4.2 conventional
>150°C
long-term stability, PC-50 / PC-51
RI > 1.50
optical clarity where required
On the line

Where this grade is used.

Representative production images of the processes these grades are specified for. The parts shown are end applications, not test data; measured values stay in the data sections above.

Coating head applying a clear liquid top coat onto a roll of film
Clear top coat on automotive filmA transparent top coat is laid on the moving film by a coating head. Cure speed and colour stability after 85 °C / 48 h are the two acceptance points at this step.
Visualised

Measured, not claimed.

Schematics of the measurement behind the figures above: the same test conditions, drawn to be read at a glance. The drawings are illustrative; the measured values are the ones stated in the data sections.

85 °C / 48 h accelerated aging: ΔE 4.2 versus ΔE 0.8ACCELERATED AGING · 85 °C / 48 H · SAME TEST RUNCONVENTIONAL KARSTEDTΔE 4.2VISIBLE YELLOWINGPC-42 · ANTI-YELLOWINGΔE 0.8NO VISIBLE COLOUR SHIFTVS80–120 °C cure window · 0.05–0.5 % dosage · PC-611 / PC-612 inhibitor
Accelerated aging comparison: ΔE 4.2 with a conventional Karstedt's catalyst against ΔE 0.8 with PC-42, both run in the same 85 °C / 48 h test and measured against an unstressed reference film. Colour patches are illustrative; the ΔE values are the measured results.
Cure kinetics with and without PC-611 inhibitorCURE KINETICS · SCHEMATIC · 100 °C CURE STEP02550751000TIMECURE DEGREE (%)100 °C CURE STEPno inhibitorwith PC-611steep risePOT LIFE AT ROOM TEMPERATURE (HOURS TO ONE WEEK)
Schematic cure kinetics, not measured data: PC-611 holds the mixed batch workable at room temperature, then cure rises steeply once the part reaches the 100 °C cure step. Read it as a comparison of curve shapes, not as a rate table.
Slot-die coating schematicSLOT-DIE COATING · SCHEMATICSLOT DIEWET FILMWEB DIRECTIONLINE SPEEDset by cure,not by the coaterCURE 15 MIN400–500 cP catalyst
Slot-die coating schematic for a release liner or PPF top coat: the die lays a wet film on the moving web, and cure happens downstream. Line speed is set by how fast the silicone cross-links, not by the coater; the 15 min cure and 400–500 cP figures are the measured values stated in the data sections.
Process window

Settings for the first trial.

Typical starting parameters for PPF & Coatings. Treat them as a trial configuration rather than a fixed recipe: the final values depend on the substrate, the equipment and the acceptance test.

ParameterGuidance
Catalyst dosage0.05%–0.5% of total compound; start at the lower bound and adjust to line speed
InhibitorPC-611 or PC-612 at 0.1%–1.0% for line stability
Cure window80–120°C depending on substrate; avoid over-cure on thin films
Coating methodSlot-die and gravure; 400–500 cP is the typical catalyst viscosity range
Mixing order

Add base and inhibitor first, then the catalyst. Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Shake the container before use, and keep drums sealed at 5–15°C away from direct light.

FAQ

Practical questions before a trial.

The questions that come up most often when this application moves from specification to a first sample run.

Which grade should we evaluate first for PPF & Coatings?

PC-42 or PC-50 is the usual starting point. Start at the lower end of the 0.05%–0.5% dosage range and confirm the cure against your own oven before adjusting.

How do we control pot life without slowing the cure?

PC-611 or PC-612 at 0.1%–1.0% for line stability. The inhibitor sets working time; the catalyst sets cure speed once the part reaches temperature. Change one of them at a time.

How does a trial move from sample to production?

Request an evaluation sample with the formulation window and acceptance test. Samples are paired with the matching inhibitor so the first trial reflects the real process; after the dosage is confirmed, supply scales from 1 kg to 5 kg and 20 kg drums with a batch COA.

Next step

Trial PPF & Coatings with a paired sample set.

Send the cure temperature, the failure you are seeing and the acceptance test. We reply with a recommended grade, platinum concentration and inhibitor pairing, plus a sample plan for the first run.

Technical reply within 24 hours
Evaluation samples in 5–7 days
COA, TDS and SDS on request
Custom concentration 1,000–20,000 PPM