PC-44
High-activity 4,000 PPM grade for automated lines that need a fast, repeatable cure onset and cannot afford start-up scrap.
Technical data.
| Platinum concentration | 4,000 PPM |
| Appearance | Colorless, transparent |
| Viscosity | 400–500 cP |
| Recommended dosage | 0.05%–0.5% of total compound |
| Packaging | 1 kg / 5 kg / 20 kg HDPE drums |
| Shelf life | 6 months, sealed at 5–15°C |
| Light sensitivity | Store sealed, away from direct light |
| Classification | Platinum complex in silicone fluid; see SDS |
Typical values. Actual performance depends on formulation, equipment and process validation. Batch COA states measured platinum content for each lot.
Why this grade.
- Fast cure onset for automated lines
- Improved resistance to sulfur and phosphorus traces
- Consistent drum-to-drum reactivity
Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Add the catalyst last, mix thoroughly, and shake the container before use.
Pair with the right inhibitor.
PC-44 is designed to be used with a precision inhibitor; the inhibitor sets the working time without slowing the hot cure.
Recommended to use with PC-611 / PC-612 / PC-617 Silicone Inhibitors for precise curing control.
| Catalyst | 0.05%–0.5% of total compound |
| Inhibitor (medium-high temp) | 0.1%–1.0% (PC-611 / 612) |
| Inhibitor (alkynol type) | 0.01%–0.20% (PC-617) |
| Mixing order | Base + inhibitor, then catalyst |
Request PC-44 samples
Evaluation quantities are available for every grade. Send your formulation window and we will confirm the recommended concentration, inhibitor pairing and sample timeline.