Battery pack seal: VOC compliance without losing compression set
A peroxide-to-addition conversion on a battery pack seal, where VOC compliance and compression set had to be met in the same production trial.
Each figure is tied to a measurement, and the result section below states the conditions that produced it. Field data and accelerated aging data are labelled separately, and the disclosure at the end of the case states how the data was obtained.
Measured, not claimed.
Schematic of the measurement behind this case: the same conditions, drawn to be read at a glance. The drawing is illustrative; the measured values are the ones stated in the result sections.
The challenge.
A battery pack seal was built on a peroxide cure system. VOC emissions failed the customer's incoming specification, and the alternative addition-cure trial produced uneven cell structure and compression set above the 10% limit.
Both failures had to be closed at once. A seal that cures evenly but sets too hard still leaks, and a seal that is soft enough but emits volatiles does not pass incoming inspection. The trial therefore had to fix cure uniformity and compression set together, in a section thick enough for cure gradients to matter.
The peroxide system also set the baseline for compression set, which is why the first addition-cure trial was judged against a 10% limit. That limit, not the VOC result, is what the alternative system failed.
The solution.
5,000 PPM platinum catalyst at 0.08% dosage, with PC-611 inhibitor to keep the mixed batch workable for the potting window.
Platinum loading set the cure speed through the section; the inhibitor set how long the batch stayed usable before the pour. The dosage was kept in the lower half of the 0.05%–0.5% range: enough activity for the section, without pushing the cure so fast that the batch gelled in the mix head.
Because the system is addition-cure, no peroxide by-products are released during cure. That is the mechanism behind the VOC result, and it is a property of the chemistry rather than of a post-cure treatment.
The result, and what produced it.
The numbers at the top of the page are the headline metrics from this case. The paragraphs here explain what produced them, with the test method and the exposure stated alongside.
Cell uniformity improved by 40% against the failed trial, and compression set came in at 8% — below the 10% limit the first addition-cure trial exceeded. Compression set was measured per the customer's internal method after 24 h at 100°C, and cell structure was read from a cured section.
The two numbers answer different questions: uniformity describes how the section cured, compression set describes how the seal behaves in service. A formulation change that improves one can move the other, which is why both are reported.
The figures describe this seal geometry, this section thickness and this cure schedule. A different section or a different contamination profile should be re-trialled rather than scaled from these numbers.
Customer production line trial; cell structure measured on cured section, compression set per customer internal method after 24 h at 100°C.
Customer production case, published with permission and without customer identification.
The grades and the application behind this case.
Every case is tied to a catalyst grade and to an application page. The grade page carries the full specification; the application page carries the process window, dosage range and inhibitor pairing for this class of part.
| Model | Pt concentration | Viscosity | Recommended dosage |
|---|---|---|---|
| PC-12 | 5,000 PPM | 400–500 cP | 0.05%–0.5% of total compound |
Open a model for packaging, shelf life, features and inhibitor pairing. Where a case names more than one grade, the solution section states which one was used in the reported trial.
Encapsulation
Stable cure where the chemistry fights back.
Anti-poisoning catalysis for potting, encapsulation and high-voltage insulation, where contaminants and thick sections defeat ordinary catalysts.
Other problems, measured the same way.
Each case is structured identically, so the challenge, solution and result can be compared across industries with the same reading discipline.
Medical LSR diaphragm: 100 steam cycles without yellowing
A respiratory valve diaphragm had to survive repeated 121°C wet-heat sterilisation without visible colour change. With the incumbent catalyst, yield after sterilisation was 82% and rejected parts were discoloured.
Mini LED encapsulation: 99.82% transmittance at 95% yield
A high-refractive-index encapsulation compound clouded when the catalyst was added, and the resulting light scattering failed the transmittance target. Yield was limited by optical rejects rather than by the dispenser.
MLCC release film: 15-minute cure, +12% yield
The coater could not reach the surface roughness target of 0.2 μm at production speed because the silicone layer was not fully cross-linked when the film was wound.
Run a comparable trial on your own line.
Send the part, the failure and the acceptance test. We will send evaluation samples of the grade used in this case, paired with the matching inhibitor, and confirm the starting dosage for your cure window.