Refractive index above 1.50, zero haze.
High-refractive-index catalysts for Mini LED encapsulation, optical bonding and electronic protective films.
Where the process breaks down.
In a high-refractive phenyl system the catalyst has two jobs: it has to cure the compound, and it has to dissolve completely and stay dissolved. A catalyst that is only partly compatible does not fail visibly in the mixing vessel. It forms a micro-dispersion that scatters light and shows up as haze in the cured part.
That distinction matters for Mini LED encapsulation, where the acceptance test is transmittance after cure and the yield limit is optical rather than mechanical. Trace catalyst residue, entrained air and precipitation all reduce the same number, so the formulation and the dispensing process have to be controlled together.
What the defect looks like.
- Catalyst is insoluble in high-RI systems and clouds the compound
- Trace catalyst residue scatters light and shows as haze under test
- Mini LED encapsulation needs high transmittance at high yield, not just one of the two
What the formulation needs.
GZ-5 is the high-RI grade: refractive index above 1.50, complete molecular solubility, zero turbidity and zero precipitation. It pairs with GZ-612 or GZ-617 inhibitors to control cure in phenyl systems.
GZ-5 is formulated for this window: refractive index above 1.50, complete molecular solubility, zero turbidity and zero precipitation, at 400–800 cP for high-RI systems. It is paired with GZ-612 or GZ-617 inhibitors designed not to cloud the optical compound.
On the line, vacuum defoaming before encapsulation removes entrained air, which otherwise reads as haze in the same transmittance measurement. Catalyst dosage stays in the 0.05%–0.5% range typical of the range, set against the cure window of the phenyl system.
How the first evaluation is run.
- Start from GZ-5 unless the failure mode points to another grade.
- Hold catalyst dosage at the lower bound of 0.05%–0.5% and fix the inhibitor dose.
- Run the customer acceptance test on the cured part, not on the liquid mix.
- Change one variable per run: grade, dosage or inhibitor.
What the numbers behind this page show.
Where this grade is used.
Representative production images of the processes these grades are specified for. The parts shown are end applications, not test data; measured values stay in the data sections above.

Measured, not claimed.
Schematics of the measurement behind the figures above: the same test conditions, drawn to be read at a glance. The drawings are illustrative; the measured values are the ones stated in the data sections.
Grades most often specified for Optical & Electronics.
Each card opens the grade page with full specification, packaging, shelf life and inhibitor pairing. Evaluation quantities are available across the range; the one exception is stated below.
Custom (1,000–20,000 PPM)
High-refractive-index catalyst for phenyl and high-RI silicone systems. RI above 1.50, complete molecular solubility, zero turbidity or precipitation. The grade behind our Mini LED encapsulation data.
5,000 PPM
The anti-yellowing benchmark. Under 85°C / 48 h accelerated aging, PC-42 holds ΔE 0.8 against 4.2 for a conventional Karstedt's catalyst. Specified into premium PPF top coats, optical films and any coating judged by colour after heat exposure.
4,000 PPM-1
A batch-controlled 4,000 PPM grade for high-precision coating lines. The -1 suffix denotes the tight-tolerance batch configuration used where coat weight and cure are measured, not estimated.
Settings for the first trial.
Typical starting parameters for Optical & Electronics. Treat them as a trial configuration rather than a fixed recipe: the final values depend on the substrate, the equipment and the acceptance test.
| Parameter | Guidance |
|---|---|
| Catalyst dosage | 0.05%–0.5% of total compound |
| Inhibitor | GZ-612 for low-to-medium temperature, GZ-617 for higher temperature |
| Mixing | Vacuum defoaming before encapsulation; GZ-5 is fully soluble |
| Cure | Verify transmittance after cure, not only before |
Add base and inhibitor first, then the catalyst. Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Shake the container before use, and keep drums sealed at 5–15°C away from direct light.
How this looks on a production line.
Measured outcomes for this application, with the challenge and the test conditions stated. Results are customer production data where noted; accelerated aging results name the comparison catalyst.
Practical questions before a trial.
The questions that come up most often when this application moves from specification to a first sample run.
Which grade should we evaluate first for Optical & Electronics?
GZ-5 or PC-42 is the usual starting point. Start at the lower end of the 0.05%–0.5% dosage range and confirm the cure against your own oven before adjusting.
How do we control pot life without slowing the cure?
GZ-612 for low-to-medium temperature, GZ-617 for higher temperature. The inhibitor sets working time; the catalyst sets cure speed once the part reaches temperature. Change one of them at a time.
How does a trial move from sample to production?
Request an evaluation sample with the formulation window and acceptance test. Samples are paired with the matching inhibitor so the first trial reflects the real process; after the dosage is confirmed, supply scales from 1 kg to 5 kg and 20 kg drums with a batch COA.
Trial Optical & Electronics with a paired sample set.
Send the cure temperature, the failure you are seeing and the acceptance test. We reply with a recommended grade, platinum concentration and inhibitor pairing, plus a sample plan for the first run.