Advanced Anti-Poisoning Catalysts
Catalyst poisoning is one of the least visible causes of a non-curing batch. PC-18B is the first-generation grade for environments with slight to moderate poisoning agents, and PC-18A is the second generation, engineered against high concentrations and multiple contaminant types. PC-18A is under final R&D and available for evaluation samples only.
Grades in this family.
| Model | Pt concentration | Appearance / viscosity | Recommended dosage | Status |
|---|---|---|---|---|
| PC-18B | Custom (1,000–20,000 PPM) | Colorless, transparent, 400–500 cP | 0.05%–0.5% of total compound | Available |
| PC-18A | Custom (1,000–20,000 PPM) | Colorless, transparent, 400–500 cP | Evaluation quantities only | R&D · sample |
Add 0.05%–0.5% of total compound mass as a starting point; adjust against line speed, section thickness and inhibitor dosage. Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Shake before use.
Choose by concentration.
Custom (1,000–20,000 PPM)
First-generation anti-poisoning catalyst. Retains stable vulcanisation activity in environments with slight to moderate poisoning impurities — trace sulfur, phosphorus and nitrogen compounds.
Custom (1,000–20,000 PPM)
Second-generation anti-poisoning catalyst, engineered against high concentrations and multiple contaminant types. Under final R&D: available for evaluation samples, with commercial supply not yet committed.
Complete the curing system.
The catalyst sets the cure speed; the inhibitor sets how long the batch stays workable. Keep the mixed batch workable through the potting window; identify the contamination source before raising dosage.
Recommended to use with PC-611 / PC-612 Silicone Inhibitors for precise curing control.
Not sure about the ratio? Send your cure temperature and target bath life — we will return a starting dosage for both components.
Where this family is used.
Open an application page for process parameters, field data and the recommended grade set.
How do I know which Advanced Anti-Poisoning grade fits my line?
Start from the concentration band your current formulation uses, then confirm cure speed and colour against a sample. If you do not have a current reference, send your line speed, cure temperature and section thickness for a recommendation.
Can I get a custom concentration in this family?
Yes. Concentrations from 1,000 to 20,000 PPM are supplied to order; the batch COA states the measured platinum content.
What documentation is supplied?
A TDS per grade, an SDS in the requested language, a batch COA and a RoHS/REACH compliance statement on request.
Request a sample or get a quote
Tell us the grade, target PPM and application. Our technical team replies within 24 hours with a recommended grade and sample lead time.