High-Activity & Anti-Poisoning Catalysts
PC-41 to PC-46 mirror the standard concentration grades but with enhanced catalytic activity and improved resistance to substrate contaminants. They are the practical choice when a line runs below ideal conditions — recycled filler, variable cure ovens, long pot life between mixing and shaping — and curing failures are costing yield rather than indicating a formulation fault.
Grades in this family.
| Model | Pt concentration | Appearance / viscosity | Recommended dosage | Status |
|---|---|---|---|---|
| PC-41 | 1,500 PPM | Colorless, transparent, 400–500 cP | 0.05%–0.5% of total compound | Available |
| PC-43 | 3,000 PPM | Colorless, transparent, 400–500 cP | 0.05%–0.5% of total compound | Available |
| PC-44 | 4,000 PPM | Colorless, transparent, 400–500 cP | 0.05%–0.5% of total compound | Available |
| PC-45 | 2,000 PPM | Colorless, transparent, 400–500 cP | 0.05%–0.5% of total compound | Available |
| PC-46 | 4,000 PPM-1 | Colorless, transparent, 400–500 cP | 0.05%–0.5% of total compound | Available |
Add 0.05%–0.5% of total compound mass as a starting point; adjust against line speed, section thickness and inhibitor dosage. Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Shake before use.
Choose by concentration.
1,500 PPM
The 1,500 PPM high-activity grade: standard-range platinum loading with upgraded catalytic performance and better tolerance of substrate contaminants.
3,000 PPM
High-activity grade at 3,000 PPM, used where an existing 3,000 PPM formulation is fast enough on paper but not in the plant.
4,000 PPM
High-activity 4,000 PPM grade for automated lines that need a fast, repeatable cure onset and cannot afford start-up scrap.
2,000 PPM
The 2,000 PPM high-activity grade for moulding shops whose cure is borderline: standard activity is technically sufficient, but yield improves with more robust kinetics.
4,000 PPM-1
Batch-controlled high-activity 4,000 PPM grade for precision coating lines, matching the PC-16 tolerance profile with enhanced kinetics.
Complete the curing system.
The catalyst sets the cure speed; the inhibitor sets how long the batch stays workable. Same inhibitor window as the standard series, with better cure stability where the substrate is contaminated.
Recommended to use with PC-611 / PC-612 / PC-617 Silicone Inhibitors for precise curing control.
Not sure about the ratio? Send your cure temperature and target bath life — we will return a starting dosage for both components.
Where this family is used.
Open an application page for process parameters, field data and the recommended grade set.
How do I know which High-Activity Series grade fits my line?
Start from the concentration band your current formulation uses, then confirm cure speed and colour against a sample. If you do not have a current reference, send your line speed, cure temperature and section thickness for a recommendation.
Can I get a custom concentration in this family?
Yes. Concentrations from 1,000 to 20,000 PPM are supplied to order; the batch COA states the measured platinum content.
What documentation is supplied?
A TDS per grade, an SDS in the requested language, a batch COA and a RoHS/REACH compliance statement on request.
Request a sample or get a quote