Applications / Medical

Addition cure with no by-products.

Platinum-catalysed, VOC-free systems for medical tubing, respiratory valves, baby teats and bakeware.

MedicalPC-42 · PC-12 · PC-51 Process data included
Failure mode

Where the process breaks down.

Medical and food-contact parts are specified by what the material releases and how it survives sterilisation. Peroxide cure leaves by-products that fail that review, which is why addition-cure platinum systems are the default for tubing, respiratory valves, teats and bakeware. Switching systems, however, exposes the next failure: colour and yield after repeated steam cycles.

With the wrong catalyst, clear silicone turns yellow through 121°C wet-heat sterilisation, and the loss shows up at the end of the process after the expensive moulding work is complete. Yield, not tensile strength, is usually what moves first.

Symptoms on the line

What the defect looks like.

  • Peroxide systems release by-products that fail medical and food-contact review
  • Repeated steam sterilisation turns clear silicone yellow
  • Yield drops at the sterilisation step, after the expensive moulding work is done
Solution

What the formulation needs.

Addition-cure platinum systems release no by-products and comply with RoHS and REACH. PC-42 holds colour through repeated 121°C steam cycles; the high-activity grades protect yield on injection lines.

PC-42 holds colour through repeated 121°C cycles; the high-activity grades protect yield on injection lines where cycle time is short. The system releases no by-products during cure, and the compliance statement is limited to what can be documented: compliant with RoHS and REACH.

Sterilisation performance has to be validated on the part rather than assumed from a catalyst datasheet. A trial normally runs the full cycle count and checks yellowness index and mechanical properties at the end, because that is the point at which the part is accepted or rejected.

Regulatory scope

Compliance documentation for the catalyst covers RoHS and REACH only. Medical case data on this site describes customer-validated field cases, and the FDA Class II reference in that case describes the end-device category. It is not a certification or approval of the catalyst.

Trial plan

How the first evaluation is run.

  • Start from PC-42 unless the failure mode points to another grade.
  • Hold catalyst dosage at the lower bound of 0.05%–0.5% and fix the inhibitor dose.
  • Run the customer acceptance test on the cured part, not on the liquid mix.
  • Change one variable per run: grade, dosage or inhibitor.
Field data

What the numbers behind this page show.

YI ≤ 1.5
after 100 × 121°C wet-heat sterilisation
82% → 98%
line yield, medical LSR diaphragms
VOC-free
no by-products, RoHS & REACH compliant
On the line

Where this grade is used.

Representative production images of the processes these grades are specified for. The parts shown are end applications, not test data; measured values stay in the data sections above.

Clear liquid silicone rubber moulded parts in an aluminium mould
Moulded LSR parts for medical devicesValve diaphragms, seals and other liquid silicone mouldings are cured with a platinum addition system. Sterilisation and biocompatibility testing belong to the finished device, not to the catalyst.
Visualised

Measured, not claimed.

Schematics of the measurement behind the figures above: the same test conditions, drawn to be read at a glance. The drawings are illustrative; the measured values are the ones stated in the data sections.

Sterilisation comparison, YI ≤ 1.5STERILISATION · 121 °C × 100 CYCLES · SCHEMATICYELLOWEDCONVENTIONAL KARSTEDTvisible yellowingYI ≤ 1.5PC-42 / PC-50 SYSTEMno visible colour shiftCUSTOMER FIELD RESULT · YIELD 82% → 98%
Sterilisation comparison schematic for an LSR medical diaphragm: 100 cycles of 121 °C wet-heat steam, conventional system on the left and the PC-42 / PC-50 system on the right. YI ≤ 1.5 and the 82 % → 98 % yield are customer field results; the swatches are illustrative.
Process window

Settings for the first trial.

Typical starting parameters for LSR Medical/Food. Treat them as a trial configuration rather than a fixed recipe: the final values depend on the substrate, the equipment and the acceptance test.

ParameterGuidance
Catalyst dosage0.05%–0.5% of total compound
InhibitorPC-613 / 614 for ambient handling, PC-611 / 612 for hot cure
SterilisationValidate colour and mechanical properties after 100 cycles
ComplianceRoHS and REACH statements available on request
Mixing order

Add base and inhibitor first, then the catalyst. Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Shake the container before use, and keep drums sealed at 5–15°C away from direct light.

FAQ

Practical questions before a trial.

The questions that come up most often when this application moves from specification to a first sample run.

Which grade should we evaluate first for LSR Medical/Food?

PC-42 or PC-12 is the usual starting point. Start at the lower end of the 0.05%–0.5% dosage range and confirm the cure against your own oven before adjusting.

How do we control pot life without slowing the cure?

PC-613 / 614 for ambient handling, PC-611 / 612 for hot cure. The inhibitor sets working time; the catalyst sets cure speed once the part reaches temperature. Change one of them at a time.

Is the catalyst approved for medical or food-contact use?

No. Medical and food-contact compliance is assessed on the finished device or article, not on the catalyst. The catalyst is supplied with RoHS and REACH statements. The medical case on this site is a customer-validated field case, and its FDA Class II reference describes the end-device category only.

Next step

Trial LSR Medical/Food with a paired sample set.

Send the cure temperature, the failure you are seeing and the acceptance test. We reply with a recommended grade, platinum concentration and inhibitor pairing, plus a sample plan for the first run.

Technical reply within 24 hours
Evaluation samples in 5–7 days
COA, TDS and SDS on request
Custom concentration 1,000–20,000 PPM