PC-611
The default inhibitor for medium-to-high temperature cure systems. Buys bench and line time without slowing the cure once the part reaches temperature.
Cure behaviour.
| Cure behaviour | Cure initiates above 80°C and accelerates rapidly above 100°C. Pot life at room temperature from a few hours up to one week. |
| Appearance | Colorless viscous liquid, 300–500 cP, nearly odourless |
| Recommended dosage | 0.1%–1.0% |
| Classification | See SDS; alkynol grades are non-hazardous |
Why use PC-611.
- Cure above 80°C
- Room-temperature pot life of hours to one week
- Nearly odourless
Start at the lower end of the dosage range and increase in steps. Over-dosage shows as a soft or tacky cure; under-dosage shows as a short bath life or scorch in the mixing vessel.
Catalyst pairing.
PC-611 is supplied as part of a complete curing system. We recommend trialling it with the catalysts below so the ratio reflects your actual process window.
Request a paired sample set.
We ship the inhibitor together with the catalyst grade so the first lab trial is representative of your production ratio.
Other inhibitors.
Medium-to-high temperature
For plants that need a full week of pot life and still want the same hot cure. Same dosage window as PC-611, longer open time.
Ambient / low temperature
For ambient-cure systems and heat-sensitive substrates. Lets the compound cure in minutes to hours at room temperature without an oven.
Ambient / low temperature
Ambient-cure inhibitor with a longer hold and lower viscosity than PC-613, for formulations that need more working time at room temperature.
Request a sample or get a quote
Tell us the grade, target PPM and application. Our technical team replies within 24 hours with a recommended grade and sample lead time.