Standard Series

PC-11

The general-purpose grade. 1,500 PPM is the most widely used concentration for large-volume silicone compounding, where a predictable cure at moderate catalyst cost matters more than speed.

Available · production grade1,500 PPM400–500 cP
PC-11 · 1,500 PPMLot-traceable
Specification

Technical data.

Platinum concentration1,500 PPM
AppearanceColorless, transparent
Viscosity400–500 cP
Recommended dosage0.05%–0.5% of total compound
Packaging1 kg / 5 kg / 20 kg HDPE drums
Shelf life6 months, sealed at 5–15°C
Light sensitivityStore sealed, away from direct light
ClassificationPlatinum complex in silicone fluid; see SDS

Typical values. Actual performance depends on formulation, equipment and process validation. Batch COA states measured platinum content for each lot.

Performance

Why this grade.

  • Lowest platinum loading in the standard range, best catalyst cost per tonne
  • Stable batch-to-batch reactivity for repeat compounding
  • Works with PC-611 / 612 / 617 inhibitors for pot-life control
Formulation note

Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Add the catalyst last, mix thoroughly, and shake the container before use.

Complete the system

Pair with the right inhibitor.

PC-11 is designed to be used with a precision inhibitor; the inhibitor sets the working time without slowing the hot cure.

Recommended to use with PC-611 / PC-612 / PC-617 Silicone Inhibitors for precise curing control.

Dosage guidance
Catalyst0.05%–0.5% of total compound
Inhibitor (medium-high temp)0.1%–1.0% (PC-611 / 612)
Inhibitor (alkynol type)0.01%–0.20% (PC-617)
Mixing orderBase + inhibitor, then catalyst
Related grades

Other Standard Series options.

ModelPt concentrationViscosityStatus
PC-125,000 PPM400–500 cPAvailableView
PC-133,000 PPM400–500 cPAvailableView
PC-144,000 PPM400–500 cPAvailableView
PC-152,000 PPM400–500 cPAvailableView
PC-164,000 PPM-1400–500 cPAvailableView
Next step

Request PC-11 samples

Evaluation quantities are available for every grade. Send your formulation window and we will confirm the recommended concentration, inhibitor pairing and sample timeline.

Technical reply within 24 hours
Evaluation samples in 5–7 days
COA, TDS and SDS on request
Custom concentration 1,000–20,000 PPM