GZ-5
High-refractive-index catalyst for phenyl and high-RI silicone systems. RI above 1.50, complete molecular solubility, zero turbidity or precipitation. The grade behind our Mini LED encapsulation data.
Technical data.
| Platinum concentration | Custom (1,000–20,000 PPM) |
| Appearance | Colorless, transparent |
| Viscosity | 400–800 cP |
| Recommended dosage | 0.05%–0.5% of total compound |
| Packaging | 1 kg / 5 kg HDPE drums |
| Shelf life | 6 months, sealed at 5–15°C |
| Light sensitivity | Store sealed, away from direct light |
| Classification | Platinum complex in silicone fluid; see SDS |
Typical values. Actual performance depends on formulation, equipment and process validation. Batch COA states measured platinum content for each lot.
Why this grade.
- Refractive index above 1.50
- Complete solubility, zero turbidity, zero precipitation
- 400–800 cP for high-RI systems
- Paired with GZ-612 / GZ-617 inhibitors
Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Add the catalyst last, mix thoroughly, and shake the container before use.
Pair with the right inhibitor.
GZ-5 is designed to be used with a precision inhibitor; the inhibitor sets the working time without slowing the hot cure.
Recommended to use with GZ-612 / GZ-617 Silicone Inhibitors for precise curing control.
| Catalyst | 0.05%–0.5% of total compound |
| Inhibitor (medium-high temp) | 0.1%–1.0% (PC-611 / 612) |
| Inhibitor (alkynol type) | 0.01%–0.20% (PC-617) |
| Mixing order | Base + inhibitor, then catalyst |
Other Optical Grade options.
| Model | Pt concentration | Viscosity | Status |
|---|
Request GZ-5 samples
Evaluation quantities are available for every grade. Send your formulation window and we will confirm the recommended concentration, inhibitor pairing and sample timeline.