Anti-Yellowing Series

PC-42

The anti-yellowing benchmark. Under 85°C / 48 h accelerated aging, PC-42 holds ΔE 0.8 against 4.2 for a conventional Karstedt's catalyst. Specified into premium PPF top coats, optical films and any coating judged by colour after heat exposure.

Available · production grade5,000 PPM300–500 cP
PC-42 · 5,000 PPMLot-traceable
Specification

Technical data.

Platinum concentration5,000 PPM
AppearanceColorless, transparent
Viscosity300–500 cP
Recommended dosage0.05%–0.5% of total compound
Packaging1 kg / 5 kg / 20 kg HDPE drums
Shelf life6 months; up to 12 months for selected modified grades
Light sensitivityStore sealed, away from direct light
ClassificationPlatinum complex in silicone fluid; see SDS

Typical values. Actual performance depends on formulation, equipment and process validation. Batch COA states measured platinum content for each lot.

Performance

Why this grade.

  • ΔE 0.8 versus 4.2 for conventional catalyst (85°C / 48 h)
  • Long-term colour hold below 100°C
  • Optical-grade clarity for PPF top coats
  • Recommended with PC-611 / 612 / 617 inhibitors
Formulation note

Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Add the catalyst last, mix thoroughly, and shake the container before use.

Complete the system

Pair with the right inhibitor.

PC-42 is designed to be used with a precision inhibitor; the inhibitor sets the working time without slowing the hot cure.

Recommended to use with PC-611 / PC-612 Silicone Inhibitors for precise curing control.

Dosage guidance
Catalyst0.05%–0.5% of total compound
Inhibitor (medium-high temp)0.1%–1.0% (PC-611 / 612)
Inhibitor (alkynol type)0.01%–0.20% (PC-617)
Mixing orderBase + inhibitor, then catalyst
Related grades

Other Anti-Yellowing Series options.

ModelPt concentrationViscosityStatus
PC-50Custom (1,000–20,000 PPM)5–50 cPAvailableView
PC-51Custom (1,000–20,000 PPM)5–50 cPAvailableView
Next step

Request PC-42 samples

Evaluation quantities are available for every grade. Send your formulation window and we will confirm the recommended concentration, inhibitor pairing and sample timeline.

Technical reply within 24 hours
Evaluation samples in 5–7 days
COA, TDS and SDS on request
Custom concentration 1,000–20,000 PPM