Optical Grade High-Refractive-Index Catalysts
GZ-5 is formulated for high-refractive and phenyl silicone systems, where a conventional catalyst can cloud the compound or drop out of solution. Refractive index above 1.50, 400–800 cP, and a fully soluble profile make it the standard choice for Mini LED encapsulation and optical bonding.
Grades in this family.
| Model | Pt concentration | Appearance / viscosity | Recommended dosage | Status |
|---|---|---|---|---|
| GZ-5 | Custom (1,000–20,000 PPM) | Colorless, transparent, 400–800 cP | 0.05%–0.5% of total compound | Available |
Add 0.05%–0.5% of total compound mass as a starting point; adjust against line speed, section thickness and inhibitor dosage. Do not allow direct contact with hydrogen-containing silicone oil or pure inhibitor before mixing. Shake before use.
Complete the curing system.
The catalyst sets the cure speed; the inhibitor sets how long the batch stays workable. Optical modifiers designed for high-refractive systems, so the inhibitor does not cloud the compound.
Recommended to use with GZ-612 / GZ-617 Silicone Inhibitors for precise curing control.
Not sure about the ratio? Send your cure temperature and target bath life — we will return a starting dosage for both components.
Where this family is used.
Open an application page for process parameters, field data and the recommended grade set.
How do I know which Optical Grade grade fits my line?
Start from the concentration band your current formulation uses, then confirm cure speed and colour against a sample. If you do not have a current reference, send your line speed, cure temperature and section thickness for a recommendation.
Can I get a custom concentration in this family?
Yes. Concentrations from 1,000 to 20,000 PPM are supplied to order; the batch COA states the measured platinum content.
What documentation is supplied?
A TDS per grade, an SDS in the requested language, a batch COA and a RoHS/REACH compliance statement on request.
Request a sample or get a quote
Tell us the grade, target PPM and application. Our technical team replies within 24 hours with a recommended grade and sample lead time.