Application article

Anti-yellowing catalyst for PPF: what the ΔE data actually shows

ΔE 0.8 against 4.2 after 48 hours at 85°C — how the test is run, what it does and does not predict, and how to reproduce it.

Application 6 min read5 September 2026

After 48 hours at 85°C, PC-42 measures a colour difference of 0.8 against 4.2 for a conventional Karstedt's catalyst. The number is quoted often enough that it is worth explaining exactly what the test does, what it predicts and what it cannot promise. A ΔE result is only meaningful when the conditions are stated: the aging temperature, the dwell time, the film thickness and the reference used for comparison.

What ΔE measures

ΔE is the numerical distance between two colours in a defined colour space. In the PPF test, one film is aged and compared with an unstressed reference made from the same batch. A low value means the aged film still reads as the same colour; a high value means the shift is noticeable. A ΔE of 4.2 after 48 hours at 85°C is not a subtle laboratory difference — it is the kind of change a customer notices on a horizontal panel.

How the test is run

  1. Cast films from the same formulation, drawdown thickness and cure schedule.
  2. Measure the baseline colour of the unstressed reference.
  3. Age the stressed film at 85°C for 48 hours.
  4. Cool and condition the film, then measure it against the reference.
  5. Run the comparison catalyst and the incumbent in the same session, on the same instrument.

The last step is the one that gets dropped. A ΔE comparison across two labs, two instruments or two weeks is not a like-for-like comparison, and the difference between 0.8 and 4.2 can disappear into the setup.

What the test does and does not predict

  • It predicts short-term heat-induced yellowing under a defined accelerated condition.
  • It does not predict years of combined solar UV, engine-bay heat and chemical exposure; those require weathering tests on the finished film.
  • It does not measure adhesion, elongation or the mechanical properties of the cured coat.
  • It says little about long-term exposure above 100°C. For top coats that run hotter, PC-50 and PC-51 extend the thermal envelope, with stability above 150°C.

The choice of grade follows from that distinction. PC-42 is the anti-yellowing benchmark for colour judged after heat exposure below 100°C. PC-50 and PC-51 are specified where the part itself runs hot and the film must retain its properties at higher temperature, not only its colour.

Common ways to get a misleading result

  • Aged and reference films cut from different batches, or coated at different thickness.
  • Reference film stored next to the oven and exposed to the same heat.
  • Colour measured before the film has cooled and stabilised.
  • A single measurement point at the film edge, where colour shifts first.
  • Incumbent catalyst tested at a different catalyst loading.

Reproducing it in your lab

Use the same base, the same inhibitor pairing and the same cure schedule for both catalysts, and change only the catalyst. Prepare duplicate films so that a handling error does not become a result. Age in a calibrated oven with the samples on the same shelf, then measure at the centre of the film and at one edge. Report the conditions with the number — 85°C, 48 hours, which reference, which instrument — so a second run can be compared.

State the conditions or the number means nothing

ΔE 0.8 versus 4.2 is a valid comparison only within one test run, on one instrument, against the same unstressed reference. Ask for the test conditions before accepting a colour claim.

For a PPF top coat, the practical question is not which catalyst has the lower number in a data sheet. It is whether the finished film still matches the reference after the heat exposure your warranty period implies. A sample trial with your own film construction answers that faster than any single figure. For a warranty discussion, the useful evidence is the same test run against the same reference, documented with the film construction and the measurement method.

Next step

From article to evaluation sample

If this article describes your process, request a sample of the recommended grade with the matching inhibitor. Evaluation quantities ship in 5–7 days.

Technical reply within 24 hours
Evaluation samples in 5–7 days
COA, TDS and SDS on request