Technical article

Platinum catalyst PPM: how to choose between 1,000 and 20,000

Concentration is not a quality grade. A practical way to select PPM from line speed, section thickness and inhibitor dosage.

Technical 4 min read27 August 2026

Platinum concentration is the most quoted and least understood number on a catalyst data sheet. A 5,000 PPM grade is not better than a 1,500 PPM grade; it simply delivers more active platinum per kilogram of catalyst. Choosing a band is a process decision: how fast the compound must cross-link, how thick the section is, and how much inhibitor is holding the reaction back before the part reaches temperature.

Concentration is not a quality grade

Every grade in a concentration ladder starts from the same Karstedt's chemistry. What changes is the amount of active platinum in the supplied liquid, and therefore how much catalyst must be weighed into the compound to deliver a given platinum load. A higher concentration lets you use less catalyst liquid; it does not automatically make the compound faster, cleaner or more stable. Those properties come from the chemistry and the rest of the formulation.

Three inputs set the band

Line speed and cycle time

A line that needs cross-linking to start quickly, or a moulding cycle measured in seconds, pushes the choice toward a higher concentration or a higher-activity grade. A slow, thick-section process can use a lower band and save catalyst cost without losing output.

Section thickness

Thick sections retain heat and cure more slowly at the core, so they need a cure that keeps going once it starts. Very thin films are the opposite problem: they can dry or cross-link before the coating has levelled, and the cure window matters more than raw speed.

Inhibitor dosage

The inhibitor holds the catalyst dormant until the part reaches its activation window. If more inhibitor is used to extend bath life, more platinum may be needed to keep the same cure once the part heats. Concentration and inhibitor dosage are chosen together, not one after the other.

The practical bands

The standard range covers the most common bands. Use the table as a starting point, then confirm it with a trial on your own line.

BandTypical useTrade-off
1,500–2,000 PPMLarge-volume compounding, industrial moulding, cost-sensitive formulationsLowest catalyst cost; slowest cross-linking in the standard range
3,000–4,000 PPMBalanced moulding and coating; matching an existing formulationModerate cost; a small step between the economy and fast grades
5,000 PPMInjection, rapid cure and high-speed coatingFastest standard cure; highest catalyst cost per tonne
Custom 1,000–20,000 PPMThin films, unusual cycles, formulations being re-engineeredRequires a validated dosage and a check on inhibitor balance

How to move between grades

Do not jump from one end of the ladder to the other. If the concentration doubles and the dosage is left unchanged, the platinum load doubles and the cure will be faster than the line or the inhibitor was built for. The reverse is equally common: a team moves to a lower concentration to save cost, keeps the old dosage, and reports that the new grade does not cure. Hold the delivered platinum load constant when comparing grades, then adjust dosage and inhibitor together.

A useful rule for trials is to change one variable per run. If concentration and inhibitor dosage move at the same time, the result cannot tell you which change caused the improvement or the failure.

Dosage matters as much as the label

The recommended catalyst dosage is 0.05%–0.5% of the total compound. The lower end suits high-activity grades and simple sections; the upper half is used with anti-poisoning grades or contaminated substrates. Weigh the catalyst rather than estimating it, and record the actual number in the batch sheet. A formulation that is validated at one dosage and run at another is a different formulation, even when the drum label is identical.

Custom concentration is a band, not a premium grade

Anything between 1,000 and 20,000 PPM can be supplied to order. Custom concentration is a way to match the platinum load to the process, not a claim that the grade performs better than the standard ladder.

The reliable approach is to request a sample at the band you believe is right, plus the neighbouring grade, and run both against the same inhibitor dosage. The difference in cure onset and final properties then tells you which end of the ladder your process actually needs.

Next step

From article to evaluation sample

If this article describes your process, request a sample of the recommended grade with the matching inhibitor. Evaluation quantities ship in 5–7 days.

Technical reply within 24 hours
Evaluation samples in 5–7 days
COA, TDS and SDS on request
Custom concentration 1,000–20,000 PPM